The material decides how a flange behaves in service far more than the flange type does. Temperature, chloride level, sour service and cost all narrow the choice before the standard and class are selected.

We machine and forge carbon, stainless, duplex and alloy grades, and supply material certificates to EN 10204 3.1 with every shipment. The comparison below is a starting point — send the service conditions and we will confirm a grade.

Material comparison

Material Corrosion resistance Service temperature Strength Relative cost Typical service
Carbon (A105)Low−29 to 425 °CMediumLowestGeneral piping, steam, water
Low-temp (A350 LF2)Low−46 to 345 °CMediumLowCold service, LNG, refrigeration
Stainless 304/316LHigh−196 to 400 °CMediumMediumChemicals, food, marine atmosphere
Duplex 2205Very high (chlorides)−50 to 300 °CHighHighOffshore, desalination, sour service
Alloy F11/F22Mediumup to 590 °CHigh (hot)HighRefinery, high-pressure steam
Alloy F91Mediumup to 625 °CVery high (hot)HighestAdvanced steam, main steam lines

For low-temperature impact testing, sour service (NACE MR0175) or elevated-temperature creep data, send the design conditions — those cases need grade-specific verification, not a table. Send the data sheet and we will confirm the grade and the applicable pressure rating in writing.

Certificates and verification

Material certificates to EN 10204 3.1 report the actual chemical composition and mechanical results for the heat, and the heat number is stamped on the part so the certificate can be matched to the component. For stainless and alloy grades, PMI is performed before shipment to confirm the grade and detect mixed material. Where the project requires independent endorsement, 3.2 certification with third-party witnessing is available at the quotation stage. Certificates are issued for the exact heat supplied — not a generic sample from stock.

Temperature is usually the first filter

Below −29 °C, standard carbon steel loses toughness and an impact-tested grade such as A350 LF2 is required. Between ambient and about 425 °C, A105 covers most duties. Above that, creep becomes the design case and chromium-molybdenum grades — F11, F22, F91 — take over. Stainless grades sit outside this ladder: they are chosen for corrosion, and their useful temperature range is set by sensitisation or sigma-phase formation.

Material group changes the rating

ASME B16.5 assigns each material to a group, and the allowable pressure for a given class comes from that group's stress table. A Class 300 flange in carbon steel and a Class 300 flange in 316L share the same dimensions but not necessarily the same allowable pressure at temperature. That is why the material belongs on the purchase order even when the class is unchanged.

Corrosion and sour service

Chlorides decide between 304 and 316, and between 316 and duplex. Sour service (H₂S) adds a hardness limit and a material qualification under NACE MR0175 / ISO 15156 — a standard A105 flange may not comply even though the pressure rating is adequate. For these cases the material, heat treatment and hardness all have to be specified together.

What to send with the inquiry

  • Fluid, design temperature and design pressure
  • Standard, size and class or PN rating
  • Quantity per size and destination port
  • Certificate level and any NDT or third-party requirement